CHEMISCHE SAMENSTELLING
incoloy 625 spiraalslang capillaire slang
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0,1 | 20 – 23 | ≥ 58 | ≤ 5 | ≤ 0,5 | ≤ 0,5 | 8 – 10 | ≤ 1* | ≤ 0,015 | ≤ 0,015 | ≤ 0,4 | 3.15 – 4.15 | ≤ 0,4 |
(massa %)
*Indien bepaald
Volgens ASTM B444, ASME SB444, AMS 5581
Voorwaarde | Treksterkte | Opbrengststerkte | Verlenging |
minimaal, ksi | minimaal, ksi | minimaal, % | |
Graad 1 | 120 | 60 | 30 |
Graad 2 | 100 | 40 | 30 |
* Hogere sterkte-eigenschappen kunnen worden verkregen in koudgeharde toestand.
70°F | 200°F | 400°F | 600°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Dikte | pond/in3 | 0,305 | - | - | - | - | - |
Thermische expansie | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Elasticiteitsmodulus | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Poisson-verhouding | - | 0,278 | 0,28 | 0,286 | 0,29 | 0,295 | - |
Warmtegeleiding | Btu-in/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Specifieke hitte | Btu/lb·°F | 0,098 | 0,102 | 0,109 | 0,115 | 0,122 | 0,118 |
Opbrengststerkte | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Treksterkte | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 spiraalslang capillaire slang
PROCESBESCHRIJVINGStaal makenElektrische boogoven gevolgd door vacuümzuurstofontkoling (VOD) of argonzuurstofontkoling (AOD).Pijpen makenConventionele naadloze, koud afgewerkte productieprocessen voor buizen en buizen. WarmtebehandelingKan niet worden gehard door warmtebehandeling.Kan worden geleverd in gegloeide, oplossingsgegloeide of koudgeharde toestand.De uitgegloeide toestand met hogere sterkte wordt doorgaans gebruikt bij toepassingen tot 1100°F, terwijl de oplossingsgegloeide toestand wordt gebruikt in toepassingen boven 1100°F.